I did manage to get a meager amount of work done with some clay today. The second attempt at the slump mold was again a failure, but at least I think I discovered the problem this time. I couldn't get the plate off leather hard, so I decided to let it dry farther. It cracked in several places because as it dries, clay shrinks. Which is something I completely was aware of, but apparently needed a reminder. My third attempt used WD40 in order to keep it from sticking, so I should be able to remove it when the clay is leather hard.
I had never used WD40 before, but I had seen others use it. It apparently works wonders as a release agent. The clay wouldn't stick to the plate even wet, that is a big wow. I was going to try powder, but I am glad I tried this instead. I hope it finally works out. I am going to try a bowl next.